Polymer Property : Flexural Strength = 24117 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 166.28 MPa
24117 psi
ASTM D790
E-Polymers SEPAZ® N1040 Nanoclay 4% High Flow Nano Composite Resin
Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi..