Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 228.57 MPa | 33151 psi | ASTM D790 |
E-Polymers SEPAZ® N5030 Nanoclay 4%, 30% Glass Fiber Reinforced Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |