Polymer Property : Flexural Strength = 225.63 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 225.63 MPa
32725 psi
Shinil Chemical SHINCON PEI-CNT Magazine Rack
Magazine Rack is used to transfer, handle, and bake lead frame or PCB substrate in semiconductor and LED packaging assembly process. Current Metal Magazine is made of anodized aluminum which is exp..
Flexural Strength 225.63 MPa
32725 psi
Shinil Chemical SHINCON PPS Electro Conductive Polymer
SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's ..
Flexural Strength 225.63 MPa
32725 psi
Shinil Chemical SHINCON PPS-CNT LCD Rack
LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b..
Flexural Strength 225.63 MPa
32725 psi
Shinil Chemical SHINNANO PA-6 Polymer Nanocomposite Air Intake Module
SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using..