Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 223.1 MPa | 32360 psi | |
Poco Graphite SUPERSiC® Si-3C Silicon Carbide SUPERSiC that has been infiltrated with silicon and then coated with a 75 µm CVD SiC coating, sealing off the porosity.Uses: Ideal for high-temperature vacuum CVD systemsInformation provided by Poc.. |
|||
Flexural Strength | 223.1 MPa | 32360 psi | |
Poco Graphite SUPERSiC® Si-8C Silicon Carbide SUPERSiC that has been infiltrated with silicon and then coated with a 200 µm CVD SiC coatingUses: Ideal for optical and lithography componentsInformation provided by Poco Graphite |