Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 1490 MPa | 216000 psi | Transverse Rupture |
PSM Industries Ferro-TiC® C Medium Alloy Tool Steel Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Exce.. |