Polymer Property : Flexural Strength = 206000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 1420 MPa
206000 psi
China Tungsten YG4C Cemented Tungsten Carbide for Mining Purposes
For geological prospecting, coal mining, tipping of electric and air drilk; for coal bed and other homogeneous rocks such as non-silicified shale, skyline and rock salt, etc.; and for medium hard sa..
Flexural Strength 1420 MPa
206000 psi
China Tungsten YG6 Cemented Tungsten Carbide for Mining Purposes
For coring crowns, electric coal drill bits, coal cutting picks. oil cone bits and scraping knife bits used in geological prospecting, coal mining and oil well boringInformation provided by China Tu..
Flexural Strength 1420 MPa
206000 psi
China Tungsten YG6 Tungsten Carbide for Dies and Wear Part Making
For drawing of steels, non-ferrous metal and alloy bars of