Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 206.01 MPa | 29879 psi | |
Shinil Chemical SHINSTAT MS Electrostatic Control Polymer Injection Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Flexural Strength | 206.01 MPa | 29879 psi | ASTM D790 |
E-Polymers SEPAZ® LH50 PP Homopolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |