Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 2.62 MPa | 380 psi | ISO 178 |
Multibase TPSiV® 4000-80A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
Flexural Strength | 2.62 MPa | 380 psi | |
BCC Products MB 1100 Polyurethane Foam Modeling Board MB 1100 is an Olive colored rigid closed-cell polyurethane foam tooling and modeling board. MB 1100 is low density foam of approximately 10lbs/ft3 board. Easily cut using CNC machining equipment or .. |