Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 2.14 MPa | 310 psi | Parallel to thickness |
Zircar Ceramics SALI-2 Alumina Insulation SALI-2 is a premium grade rigid insulation board used as hotface insulation or a precision machined furnace fixtures.Information provided by Zircar Ceramics. |