Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 133.0 MPa
19290 psi
UNI EN ISO 14125: 2000
CRP Technology Windform® XT 2.0 Polyamide-Carbon Fiber Composite
Processed by selective laser sintering (SLS). Windform® XT 2.0 is the evolution of the ground breaking high performance Windform® XT, the carbon fiber reinforced composite material, known for its..
Flexural Strength 133.0 MPa
19290 psi
ASTM D790
Aclo Accutech SAN SAN930G40L Glass Reinforced