Polymer Property : Flexural Strength = 1900 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 1900 MPa
276000 psi
China Tungsten YT730 Tungsten Carbide
Having higher impact and heat shock resistance, for rough turning, milling and planning of carbon steel, alloy steel, hi-Mn steel, hi-strength steel and cast steel.Information provided by China Tung..
Flexural Strength 1900 MPa
276000 psi
China Tungsten YT770 Tungsten Carbide
High toughness. wear resistance and heat shock resistance. for milling and medium speed and full-feed turning of steel, cast steel, alloy steel, stainless steel and hi-Mn steelInformation provided b..