Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 124.14 MPa | 18005 psi | ASTM D790 |
Lucent Polymers GPB-FR515 Polybutylene Terephthalate, 15% Glass Fiber Reinforced, Flame Resistant Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 124.14 MPa | 18005 psi | ASTM D790 |
Lucent Polymers GPP-140 Polypropylene Homopolymer, 40% Glass Fiber Reinforced, Chemically Coupled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |