Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 18.9 MPa | 2740 psi | DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato.. |