Polymer Property : Flexural Strength = 17505 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 120.69 MPa
17505 psi
ASTM D790
Lucent Polymers GPP-240 Homopolymer Polypropylene, 40% Glass Fiber Reinforced, Chemically Coupled
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.