Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 1725 MPa | 250200 psi | Typical epoxy composite property |
Hexcel® HexTow™ AS2C Carbon Fiber HexTow™ AS2C carbon fiber is a continuous, high strength, high strain, PAN based fiber available in 3,000 (3K), 6,000 (6K), and 12,000 (12K) filament count tows. This fiber has been surface treated.. |