Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 119 MPa | 17200 psi | ASTM D790 |
Techmer ES HiFill® ABS GF20 IM 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedTPCI# 7782121Information provided by T.. |
|||
Flexural Strength | 119 MPa | 17200 psi | ASTM D790 |
Ensinger Tecapeek® XP-106 Compression Molded PEEK Compound, 40% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |