Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 17.69 MPa | 2565 psi | ASTM D580 |
Protective Coating PC-11® White Epoxy Paste PC-11® is a Heavy Duty-white epoxy Paste formulated by the manufacturer of PC-7.® After mixing, PC-11® can be applied to a dry, wet or underwater surface and will cure to an off white color. PC.. |