Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 1140 MPa | 166000 psi | Transverse Rupture |
Pacific Sintered Materials FX-232-T Infiltrated High Carbon Steel Powdered Metal Good strength, shock resistance and hardenability. Moderate tolerance control.Equivalent MPIF Specification: FX-1008-50All information provided by Pacific Sintered Metals. |
|||
Flexural Strength | 1140 MPa | 166000 psi | Transverse Rupture |
PSM Industries Pacific Sintered Metals Infiltrated High Carbon Steel FX-232-T Powdered Metal Good strength, shock resistance and hardenability, Moderate tolerance control Equivalent MPIF Specification: FX-1008-50Information Provided by Pacific Sintered Metals, a division of PSM Industries |