Polymer Property : Flexural Strength = 16146 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 111.32 MPa
16146 psi
Bulk Molding Compounds BMC T40(25)-XHS-15869 Die Casting Replacement Grade Molding Compound
BMC T40(25)-XHS-15869 is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical pro..