Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 1550 MPa | 225000 psi | Transverse Rupture |
PSM Industries Ferro-TiC® SK Impact Resistant Tool Steel Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Exce.. |
|||
Flexural Strength | 1550 MPa | 225000 psi | |
China Tungsten YG600 Tungsten Carbide High red hardness, wear resistance and thermal strength under high temperature. Machining of cast irons. quenched steel. non-ferrous metals and non-metallic materialsInformation provided by China Tu.. |