Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 104.83 MPa | 15204 psi | ASTM D790 |
Lucent Polymers GPP-230 Polypropylene, 30% Glass Fiber Reinforced, Chemically Coupled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |