Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | >= 1460 MPa | >= 212000 psi | |
China Tungsten YWR2 Tungsten Carbide with Rare Earth Additive Higher wear resistance and service strength than YW2 capable of undergoing high impact load. For roughing and Semi-finishing of heat resistant steel ,hi-Mn steel, stainless steel and high alloy stee.. |