Mechanical Properties Metric English Comments
Flexural Strength 94.80 MPa
13750 psi
ASTM D790
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Flexural Strength 94.80 MPa
13750 psi
ASTM D790
Polymer Resources AH-GP1-[color]-H Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Strength 94.80 MPa
13750 psi
ASTM D790
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, Heat Stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Flexural Strength 94.80 MPa
13750 psi
ASTM D790
Polymer Resources AH-GP2-[color]-H Acetal Homopolymer, Medium Flow, General Purpose Molding, Heat Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Strength 94.80 MPa
13750 psi
ASTM D790
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin, Heat Stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Flexural Strength 94.80 MPa
13750 psi
ASTM D790
Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Strength 94.80 MPa
13750 psi
ASTM D790
Polymer Resources PC-G5-IM Polycarbonate, 5% Glass Reinforced, Impact Modified, Foamable
Polycarbonate, 5% Glass Reinforced, Impact Modified, FoamableProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
Flexural Strength 94.80 MPa
13750 psi
ASTM D790
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Strength 94.80 MPa
13750 psi
ASTM D790
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength  (Unverified Data**)
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Strength 94.80 MPa
13750 psi
ASTM D790
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, General Purpose Molding  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.