Flexural Strength 12.8 MPa
1850 psi
ASTM D790
Techmer ES HiFill® ABS E GM30 LE 30% Glass Filled
Availability: North AmericaFeatures: Low ExtractablesForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc.