Mechanical Properties Metric English Comments
Flexural Strength 81.43 MPa
11810 psi
ASTM D790
PolyOne Therma-Tech™ ES-5500C TC-EM Polyethersulfone  (discontinued **)
Description/Features:Thermally ConductiveCeramic FilledPolyOne First ChoiceInformation provided by PolyOne Corporation.