Polymer Property : Flexural Strength = 118.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 118.7 MPa
17220 psi
Shinil Chemical SHINSTRA PA-66 W100SRB Structural Polymer Abrasion Resistance
SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog..
Flexural Strength 118.7 MPa
17220 psi
ASTM D790
E-Polymers SEPAZ® N3040IR Nanoclay 4% Impact Modified Nano Composite Resin
Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi..