Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 117.24 MPa | 17004 psi | ASTM D790 |
Lucent Polymers GPP-340 Polypropylene Homopolymer, 40% Glass Fiber Reinforced, Chemically Coupled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |