Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 117.2 MPa | 17000 psi | ASTM D790 |
Plaskolite Optix® CA-86 Clear General Purpose Acrylic Resin General purpose acrylic resin, extrusion and injection molding gradeApplications: A general-purpose acrylic resin designed for high heat application. This resin offers the highest heat resistance a.. |
|||
Flexural Strength | 117.2 MPa | 17000 psi | ASTM D790 |
Plaskolite West Optix® CA-86 Clear General Purpose Acrylic Resin General purpose acrylic resin, extrusion and injection molding gradeApplications: A general-purpose acrylic resin designed for high heat application. This resin offers the highest heat resistance a.. |