Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 116.97 MPa | 16965 psi | ISO 178 |
MRC Polymers NAXALOYâ„¢ 780 GF11 PC+PBT Polyester Blend, 11% Glass Fiber Filled Good chemical resistance, impact and heat resistanceAvailable in Black OnlyCan be UV StabilizedInternal and external lubricant can be added.Information provided by MRC Polymers Inc. |