Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 786 MPa @Temperature 23.9 °C |
114000 psi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D790 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4581 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |