Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 110.9 - 112.3 MPa | 16080 - 16290 psi | 90 Minute UV Cure + Thermal; ASTM D790 |
3D Systems Accura® SI 40 Plastic for the SLA® 250 System Accura 40 "Ar" or "Hc" type materials - for the SLA 250 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing .. |