Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 764 MPa | 111000 psi | 0° Fiber Direction |
Saint-Gobain Quartzel® Fabric/Cyanate Ester Resin Composite Fiber: Quartzel® 8 Harness Fabric Style 581. Resin 954-2A System.Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous, n.. |