Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 758 MPa @Temperature 23.9 °C |
110000 psi @Temperature 75.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f.. |
|||
Flexural Strength | 758 MPa @Temperature 23.9 °C |
110000 psi @Temperature 75.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f.. |
|||
Flexural Strength | 760 MPa | 110000 psi | |
McDanel Advanced Ceramics SiAlON Information provided by McDanel Advanced Ceramic Technologies. |
|||
Flexural Strength | 758 MPa | 110000 psi | ASTM F417 |
CoorsTek Dura-Z™ MgO Partially Stabilized Zirconia Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Flexural Strength | 760 MPa | 110000 psi | longitudinal; ISO 178 |
Bond Laminates TEPEX® dynalite 201-C200(x)/45% Carbon – PA6.6 Consolidated Composite Laminate Within the TEPEX® composite laminate, Polyamide 66 is a resin known for its high hardness, stiffness, abrasion resistance, heat and chemical resistances. The carbon used within this material is ae.. |
|||
Flexural Strength | 760 MPa | 110000 psi | |
Astro Met ZTA 96 Zirconia Toughened Alumina General Description:ZTA-96 is a zirconia toughened alumina ceramic that exhibits excellent wear and corrosion resistance along with high strength and toughness. Astro Met has developed ZTA-96 zircon.. |
|||
Flexural Strength | 758 MPa | 110000 psi | 90° stress angle |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Flexural Strength | 758 MPa | 110000 psi | 0° stress angle |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |