Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 1090 MPa | 158000 psi | Transverse Rupture |
Pacific Sintered Materials FX-227-T Infiltrated Steel Powdered Metal Machines and plates well. Good in hydraulic applications. Moderate tolerance control.Equivalent MPIF Specification: FX-1005-50All information provided by Pacific Sintered Metals. |
|||
Flexural Strength | 1090 MPa | 158000 psi | Transverse Rupture |
PSM Industries Pacific Sintered Metals Infiltrated Steel FX-227-T Powdered Metal Machines and plates well, Good in hydraulic applications, Moderate tolerance control Equivalent MPIF Specifications: FX-1005-50Information Provided by Pacific Sintered Metals, a division of PSM Ind.. |