Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 102.7 MPa | 14900 psi | ASTM D790 |
Diamond Polymers NPP30-0800 GF40 40% Glass Filled Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |