Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 0.230 MPa | 33.4 psi | 19 g/l |
Jackon JACKOCELL® S214 Expanded Polystyrene Construction and Block Molding Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S214 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces a.. |