Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 0.1642 MPa | 23.82 psi | ASTM D790 |
Sekisui PIOCELAN SP-50E Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |