Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Clash Berg Modulus | 0.565 GPa | 81.9 ksi | ASTM D1043 |
PolyOne Geon™ Vinyl Flexible A90F1 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Clash Berg Modulus | 0.565 GPa | 81.9 ksi | ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B5D02 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |