Polymer Property : Clash Berg Modulus = 80.9 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Clash Berg Modulus 0.558 GPa
80.9 ksi
ASTM D1043
PolyOne Geon™ Vinyl Flexible B5DG1 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Clash Berg Modulus 0.558 GPa
80.9 ksi
ASTM D1043
PolyOne Geon™ Vinyl Flexible B9000 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne