Mechanical Properties Metric English Comments
Clash Berg Modulus 0.00689 - 0.996 GPa
0.999 - 144 ksi
Average value: 0.477 GPa Grade Count:10
Overview of materials for PVC, Transparent
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M..
Clash Berg Modulus 0.00689 - 0.996 GPa
0.999 - 144 ksi
Average value: 0.341 GPa Grade Count:20
Overview of materials for PVC, Flexible Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat..