Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Clash Berg Modulus | 0.634 GPa | 92.0 ksi | ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B5DU0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.634 GPa | 92.0 ksi | ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B5D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |