Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 99.549 MPa @Strain 28.574 %, Temperature -40.0 °C |
14438 psi @Strain 28.574 %, Temperature -40.0 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod.. |