Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 98.89 MPa @Strain 1.13 %, Temperature 0.000 °C |
14340 psi @Strain 1.13 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66
(Unverified Data**) 40% Glass/Mineral Reinforced Polyamide 66 Zytel FE270038 is a 40% glass fiber/mineral reinforced heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.I.. |