Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 6.73 MPa @Strain 125.27 %, Temperature 120 °C |
976 psi @Strain 125.27 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET