Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 96.83 MPa @Strain 4.97 %, Temperature 0.000 °C |
14040 psi @Strain 4.97 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66
(Unverified Data**) Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du.. |