Mechanical Properties Metric English Comments
Tensile Stress 65.14 MPa

@Strain 0.940 %,
Temperature 60.0 °C
9448 psi

@Strain 0.940 %,
Temperature 140 °F
ISO 527
DuPont Performance Polymers Crastin® SK609 NC010 PBT  (Unverified Data**)
Crastin® SK609 NC010 is a 50% glass fiber reinforced, lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 65.14 MPa

@Strain 0.990 %,
Temperature 90.0 °C
9448 psi

@Strain 0.990 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G45L NC010 Nylon 6  (Unverified Data**)
45% Glass Reinforced Polyamide 6Zytel 73G45L NC010 is a 45% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers