Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 6.43 MPa @Strain 18.66 %, Temperature 150 °C |
933 psi @Strain 18.66 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010
(Unverified Data**) Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s.. |
|||
Tensile Stress | 6.43 MPa @Strain 47.23 %, Temperature 100 °C |
933 psi @Strain 47.23 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET
(Unverified Data**) 47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc.. |