Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 64.2 MPa @Strain 1.55 %, Temperature 23.0 °C |
9310 psi @Strain 1.55 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT