Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 93.28 MPa @Strain 3.61 %, Temperature 90.0 °C |
13530 psi @Strain 3.61 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G45L NC010 Nylon 6
(Unverified Data**) 45% Glass Reinforced Polyamide 6Zytel 73G45L NC010 is a 45% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |