Mechanical Properties Metric English Comments
Tensile Stress 63.6 MPa

@Strain 9.80 %,
Temperature 23.0 °C
9220 psi

@Strain 9.80 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani..
Tensile Stress 63.6 MPa

@Strain 5.00 %,
Temperature 23.0 °C
9220 psi

@Strain 5.00 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AL is a medium viscosity acetal homopolymer with an advanced system of lubrication for applications requiring ..
Tensile Stress 63.6 MPa

@Strain 9.80 %,
Temperature 23.0 °C
9220 psi

@Strain 9.80 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b..
Tensile Stress 63.6 MPa

@Strain 5.00 %,
Temperature 23.0 °C
9220 psi

@Strain 5.00 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG500AL is a medium viscosity acetal homopolymer lubricated for low wear ..
Tensile Stress 63.6 MPa

@Strain 3.00 %,
Temperature 40.0 °C
9220 psi

@Strain 3.00 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT)
10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers
Tensile Stress 63.6 MPa

@Strain 1.50 %,
Temperature 23.0 °C
9220 psi

@Strain 1.50 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT)
10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved